摘要
判断故障,分析要点。
2/5
导柱损伤,动静模侧向偏移。解决办法:模具四周增加4个圆形定位键
3/5
浇口脱料困难,原因料嘴变形损伤,或喷觜口球形太小,易碰伤。解决办法,更换唧嘴,增加拉料杆大小或深度。
4/5
动模板弯曲,或顶针板变形。解决办法,增加中托柱和塞打螺丝分布。
5/5
顶杆弯曲断裂或漏料。模温高顶杆膨胀卡死,解决办法,重做顶杆。顶杆前端预留10-15mm配合段,中间部分磨小0.2m。
咨询记录 · 回答于
F.context('wywContentAnswerPayChatList-3752449378', [{content:null,ctype:1,type:1},{content:null,ctype:1,type:2},{content:2\/5,ctype:1,type:2},{content:null,ctype:1,type:2},{content:3\/5,ctype:1,type:2},{content:null,ctype:1,type:2},{content:4\/5,ctype:1,type:2},{content:null,ctype:1,type:2},{content:5\/5,ctype:1,type:2},{content:null,ctype:1,type:2},{content:https:\/\/iknow-pic.cdn.bcebos.com\/d8f9d72a6059252d4a3c8b64249b033b5bb5b9a3?x-bce-process%3Dimage%2Fresize%2Cm_lfit%2Cw_600%2Ch_800%2Climit_1%2Fquality%2Cq_85%2Fformat%2Cf_jpg,ctype:2,type:1},{content:null,ctype:1,type:1},{content:https:\/\/iknow-pic.cdn.bcebos.com\/9213b07eca806538b9c1327387dda144ad3482a3?x-bce-process%3Dimage%2Fresize%2Cm_lfit%2Cw_600%2Ch_800%2Climit_1%2Fquality%2Cq_85%2Fformat%2Cf_jpg,ctype:2,type:2},{content:null,ctype:1,type:2}]);
塑料模具维修常见方法。
判断故障,分析要点。
2/5
导柱损伤,动静模侧向偏移。解决办法:模具四周增加4个圆形定位键
3/5
浇口脱料困难,原因料嘴变形损伤,或喷觜口球形太小,易碰伤。解决办法,更换唧嘴,增加拉料杆大小或深度。
4/5
动模板弯曲,或顶针板变形。解决办法,增加中托柱和塞打螺丝分布。
5/5
顶杆弯曲断裂或漏料。模温高顶杆膨胀卡死,解决办法,重做顶杆。顶杆前端预留10-15mm配合段,中间部分磨小0.2m。
这个修一下需要多少钱。
这个我不是这类的厂商,你可以问厂商技术员,维修费用,还包括工时费。